Skip to content
PT SCBI

Record · Quality

Drop Strength of Our Shisha Charcoal: The Drop Test on Lit Pieces and Its Log

This record belongs to the quality section and shows how this factory's shisha charcoal, the hookah charcoal or hookah coals of US and Canadian buyers, holds up when it is dropped. It is written for the importer or quality manager who wants the briquettes to reach the bowl whole. It gives the test, its pass rule and the log of each check.

Written by
Henry Sinaga
Reviewed by
Dimas Setyawan,
Updated
Reading time
3 min read

Quick answer

How strong is this factory's shisha charcoal when dropped, and how is it tested?

A piece passes when it survives 3 drops; in the check of November 12, 2026, 338 of 350 lit pieces passed and 12 broke. The test of these coconut shell charcoal briquettes drops lit pieces from 100 cm for cubes and 30 cm for hexagonal, dome and finger pieces, and a chipped piece counts as a pass.

Drop-strength log: 1 confirmed record from 2026-11-12 to 2026-11-12. Per oven load and shape.
Date BatchShapePieces droppedBrokenIntact (%)
2026-11-12Cube 26 mm3501296.6

Method: 350 lit pieces per oven load, each heated for 10 minutes and set on a shisha bowl for 5 minutes, then dropped onto a hard tiled floor from 100 cm (cubes) or 30 cm (hexagonal, dome and finger); a piece passes when it does not break in at least 3 drops, and a chipped piece counts as a pass.

Last updated 2026-11-12 · re-checked at least every 14 days · next due by 2026-11-26.

1. What drop strength is

Drop strength is how well a briquette resists breaking when it falls, and it is read from a drop test.

Definition

drop strength

Drop strength is the resistance of a charcoal briquette to breaking when it is dropped, measured as the share of pieces that stay whole in a drop test.

In this factory's test a piece passes when it does not break in at least 3 drops, and a chipped piece counts as a pass. A check counts the pieces that broke against the pieces dropped, so its result is a share of whole pieces, not a force or a hardness figure.

How facts on this page are confirmed is set out in the editorial and review policy.

2. How the drop test runs

The test uses lit pieces, 350 per oven load, each dropped from a set height onto a hard floor. The pieces are dropped lit, after 10 minutes of heating and 5 minutes on a shisha bowl.

Drop heights of the drop test of coconut shell charcoal briquettes by shape, onto a hard tiled floor, in centimeters, as stated by the owner in November 2026.
ShapeDrop height
Cube 100 cm
Hexagonal, dome and finger 30 cm

The pieces are made at the extrusion step that forms them, and cracks or breakage is one of the reasons a batch fails.

3. The drop log

The log sits at the top of this page, newest check first, with the method it is kept by and the date it was last checked.

  • Batch and shape. The batch the pieces came from, by its production date, and the shape tested.
  • Pieces dropped and broken. The count of the check.
  • Intact. The share of the pieces dropped that stayed whole, in percent.

The newest check, on November 12, 2026, dropped 350 pieces of 26 mm cubes: 12 broke and 338 passed, 96.6 % of the pieces dropped. One check tests the pieces of one oven load, so the log shows the result load by load, not a figure for every carton of a container.

4. Breakage on arrival

A drop test describes the pieces of one check; what reaches your warehouse also depends on the handling and the carton on the way.

If cartons arrive with broken pieces, photograph them with the carton marks visible before anything is moved, and follow what to do when cartons arrive with broken pieces, where pressing, drying, handling and the carton are each checked as a cause of breakage.

A claim about quality is raised within 14 days of arrival of the container at the buyer's warehouse, under the claims process. Each batch's retained sample is what a claim is set against, so name the order, and the batch if you have it, when you report the breakage.

Questions buyers ask

Does a chipped piece count as broken?
No. A chipped piece counts as a pass. A piece counts as broken when it breaks within its 3 drops.
Is there a pass mark for a batch?
None is on file. Each piece passes or fails on its own drops, and the log shows how many of the pieces in each check stayed whole: 338 of 350 in the check of November 12, 2026.

Use the data before you order

Request a sample from current production and compare it with the latest rows.