Why Shisha Charcoal Sparks: Two Likely Causes, What the Factory Does and What to Check

This page belongs to the troubleshooting guide and covers sparking in shisha charcoal, the hookah charcoal or hookah coals of US and Canadian buyers. It is written for the importer whose customers report sparks. It keeps to the two causes a published source supports and the checks that tell them apart.

Written by
Henry Sinaga
Reviewed by
Dimas Setyawan,
Updated
Reading time
4 min read
Milled shell charcoal runs through a rotary sieve in repeated cleaning passes before it is mixed with the binder.

Quick answer

Why does shisha charcoal spark, and what does this factory do about it?

Sparking can point to foreign matter or trapped moisture in a piece; the factory fails a batch that smokes or smells on warming up. The laboratory report does not measure sparking in coconut shell charcoal briquettes, so test a carton kept dry beside the one that sparked, and look for grit in the ash, before raising it within 14 days of arrival.

1. What sparking is

Sparking is seen, not measured: no result on the laboratory report records it.

Definition

sparking

Sparking, for coconut shell charcoal briquettes, is the throwing of glowing particles from a lit piece while it heats, an observation made by eye rather than a laboratory result.

The report on file states moisture, ash, volatile matter and fixed carbon, and none of them measures sparks. Sparking is judged by eye, in use or in a sample test, so its cause in a given piece is something to test, not to read off a report.

How facts on this page are confirmed is set out in the editorial and review policy.

2. Two likely causes

Two causes are checked first: foreign matter in the piece, and moisture held inside it.

Two likely causes of sparking in coconut shell charcoal briquettes, what the cited published source says about each, and what to look for; neither cause is measured on the laboratory report.
Likely causeWhat the source saysWhat to look for
Foreign matter FAO's handbook names earth and sand contamination among the causes of high ash in charcoal, and notes that charcoal fines can carry mineral sand and clay picked up from the ground.Grit or hard specks in the ash of the pieces that sparked
Moisture held in the piece FAO notes that charcoal takes up moisture from humid air quickly, and that the water must be evaporated on burning.Pieces from a damp or opened carton sparking more than pieces from a carton kept dry
Each delivery of shell charcoal is checked before milling; earth and sand are among the contaminants FAO names for charcoal.

A spark alone proves neither cause, and the device and the way a piece is lit can play a part. The checks in section 4 separate the two.

3. What the factory does against it

The factory works against both causes at intake, at the sieve, at the oven and at the batch check.

This factory's steps against foreign matter and moisture in its coconut shell charcoal briquettes, as confirmed by the owner in November 2026.
StepWhat is doneAgainst
Intake Each delivery is checked: moisture below 12%, fixed carbon 82% or more, volatile matter 14% or less, ash content and ash colorForeign matter and moisture
Milling 4 hammer mills, then a 10 m rotary sieve in 5 cleaning passesForeign matter
Drying Electric ovens, a slow cycle of 48 hours or more, to moisture of 2% at most; measured with a moisture meter on every oven loadMoisture
Weathering 14 days, under cover in the open air, after production and before packingRain on finished pieces
Batch check A batch fails on smell or smoke on warming upFaults that show as a batch heats
Packing Packed by the in-house team, who check every piece by handVisible defects
Finished briquettes rest under cover in the open air before packing.

The checks on each delivery of shell charcoal are set out in how incoming shell charcoal is checked, and drying on the drying page.

4. What to check when pieces spark

When pieces spark, four checks narrow the cause before a claim.

  1. Step 1

    Note the carton

    Which pieces. Write down the carton marks, and whether the carton was opened, damp or kept in humid air.

  2. Step 2

    Test a dry carton beside it

    Moisture first. Light pieces from a carton kept closed and dry beside pieces from the carton that sparked, on the same setup.

  3. Step 3

    Look at the ash

    Grit or not. After the burn, look for grit or hard specks in the ash of the pieces that sparked.

  4. Step 4

    Read the shipment's report

    Ash and moisture. Compare the ash and moisture on the shipment's laboratory report with the grade range and with earlier reports.

If the cause points to the charcoal, report it within 14 days of the arrival of the container at the buyer's warehouse. The route is on the troubleshooting page and the claims and remedies page, and the retained sample of the batch is what your report is compared with. Broken pieces and dust have a page of their own: breakage and dust.

Questions buyers ask

Does the laboratory report show whether a batch will spark?
No. The report states moisture, ash, volatile matter and fixed carbon, and none of them measures sparking. A high ash figure can follow from earth and sand in the charcoal, but no figure predicts sparks in a given piece.
Can sparking start after delivery?
If moisture is the cause, it can. Charcoal takes up moisture from humid air, so keep cartons closed and dry, and test pieces from a carton stored dry beside pieces from the carton that sparked.

Sources

  1. Simple technologies for charcoal making (FAO Forestry Paper 41), chapter 10: Using charcoal efficiently (opens in new tab), Food and Agriculture Organization of the United Nations — accessed
  2. Simple technologies for charcoal making (FAO Forestry Paper 41), chapter 9: Transport, storage and distribution of charcoal (opens in new tab), Food and Agriculture Organization of the United Nations — accessed

Test before you commit a container